Teknopoliderz 2K TIX is a three-component thixotropic elastomeric elastomeric polyurethane bitumen-modified polyurethane joint sealant that provides waterproofing between concrete elements.
Applications:
• For work on runways and parking lots at airports
• For jointing joints on the surface of above-ground fuel and engine oil storage areas
• For asphalt and concrete surfaces, natural stone, mosaic and sheet metal surfaces with appropriate primer.
• For work on military fields
• For filling joints between asphalt and asphalt, asphalt and concrete, concrete and concrete, with a joint filling depth of half the width and a minimum depth of 1 cm
• For filling joints of bituminous pavements with concrete pavements
• For repairing cracks in asphalt and concrete roads.
• For filling joints in parking lots, underground parking lots and car washes.
Sealant Properties:
• Easy to use
• Can be used on vertical surfaces
• Suitable for external and internal use
• Elastic
• Solvent free
• Resistant to UV rays
• Resistant to changes in weather conditions
• Resistant to various solutions, fuels and jet oil
• Polyurethane
• Conforms to technical standards TS 5926 EN 14188-2, SS-S-00200D and BS 5212
|
Name of the indicator |
Normative value |
|
Composition |
Two-component polyurethane |
|
Color |
Black |
|
Packaging |
10,3 kg |
|
Type |
Thixotropic |
|
Store in a dry, dark place, subject to a temperature range of +50C - +350C, humidity 75%. |
12 months in closed original packaging |
|
Density |
1.35 ± 0.05 kg/l |
|
Application temperature |
from + 5 °C to + 40 °C |
|
The life of the mixture |
35 - 45 minutes. |
|
Shore hardness (A) |
20 + 5 |
|
A complete set of strengths |
12 hours (with a seam depth of 1 mm) |
|
Tensile strength |
400-600% |
|
Maximum allowable deformation of the seam |
25% |
|
Volume of solid matter |
100% |
|
Elasticity |
> 90% |
| For seams |
from 10 mm |
|
Operating temperature range |
-30 °С - + 80 °С |
Instructions:
• Before applying Teknopoliderz 2K, clean the joints from dirt and all substances that prevent adhesion with compressed air and lay a sealing harness.
• To prepare the working solution, first mix component A separately using a low-speed electric mixer (500-800 rpm). Then add components B and C and mix the solution until a homogeneous mixture is obtained for at least 3 minutes.
• The mixed and ready-to-use material is applied with a sealant gun within 35 minutes.
Notes:
• It is recommended to wear work clothes and protective gloves.
• Tools and equipment used should be washed immediately after use.
• Do not use the mixture in the rain.